RE:Maybe Ucore will not be doing PMG. " Under conventional methods, it takes about 27 hours to make a rare metal solution and recover the metals from a one-square-centimeter piece of a catalyst. But the new method requires only up to 10 minutes."
Separation is still required. I think this tech could really help us get the economics of the PLS going in our favour. Great find!